A concrete slab looks solid, but it is porous and it moves water. In Florida the humid air, summer rain and high water table mean that water vapor often travels up through a slab.
Why it matters
When moisture meets a coating, a glue or a floor covering, it can lift the film, make bubbles or cause the floor to peel. The failure shows up weeks or months later and costs far more than a test.
How it is tested
- Calcium chloride test: measures how much vapor leaves the surface over a day.
- In-slab humidity probes: measure the humidity inside the concrete.
What happens next
If the numbers are within the limit for your product, the floor goes on. If not, a vapor-reducing coating can often make the slab ready, or a polish and guard can be used, which tolerate moisture better.
The Slab Moisture Check on this site compares your numbers with typical limits for each kind of floor. Always confirm with the product data sheet.
Related services
Questions about your own floor? Call or text (813) 516-3422, or use the estimate form below.